General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.3 g/cm³ Show Material materials with Densidad of 8.3 g/cm³ | Typical for Cobalt Chromium Molybdenum |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 1.5E-5 1/K | Typical for Cobalt Chromium Molybdenum |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobalto | 61 - 63 % Show Material materials with Cobalto of 61 - 63 % |
Cromo | 7.5 - 10 % Show Material materials with Cromo of 7.5 - 10 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 3 % Show Material materials with Hierro of 3 % |
Molibdeno | 26.5 - 30 % Show Material materials with Molibdeno of 26.5 - 30 % |
Níquel | 3 % Show Material materials with Níquel of 3 % |
Silicona | 2.2 - 3 % Show Material materials with Silicona of 2.2 - 3 % |