General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.75 - 8.65 g/cm³ Show Material materials with Densidad of 7.75 - 8.65 g/cm³ | Typical for Nickel Chromium Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 150 - 245 GPa Show Material materials with Módulo elástico of 150 - 245 GPa | Typical for Nickel Chromium Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Chromium Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Alloy |
Temperatura de fusión | 1400 °C Show Material materials with Temperatura de fusión of 1400 °C | Typical for Nickel Chromium Alloy |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 1.8 - 2.2 % Show Material materials with Carbono of 1.8 - 2.2 % |
Cromo | 28 - 30 % Show Material materials with Cromo of 28 - 30 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 1 - 8 % Show Material materials with Hierro of 1 - 8 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 4 - 6 % Show Material materials with Molibdeno of 4 - 6 % |
Silicona | 0.8 - 1.2 % Show Material materials with Silicona of 0.8 - 1.2 % |