Mecánica
Property | Temperature | Value |
---|---|---|
Estricción | 20.0 °C | 5 % Show Material materials with Estricción of 5 % |
760.0 °C | 23 % Show Material materials with Estricción of 23 % | |
Resistencia a la tracción | 20.0 °C | 770 MPa Show Material materials with Resistencia a la tracción of 770 MPa |
760.0 °C | 520 MPa Show Material materials with Resistencia a la tracción of 520 MPa | |
Chemical properties
Property | Value |
---|---|
Boro | 1.5E-3 % Show Material materials with Boro of 1.5E-3 % |
Carbono | 0.4 % Show Material materials with Carbono of 0.4 % |
Cromo | 19 % Show Material materials with Cromo of 19 % |
Hierro | 66 - 100 % Show Material materials with Hierro of 66 - 100 % |
Manganeso | 6.5 % Show Material materials with Manganeso of 6.5 % |
Niobio | 0.1 % Show Material materials with Niobio of 0.1 % |
Níquel | 8 % Show Material materials with Níquel of 8 % |