General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Dureza Rockwell C | 23.0 °C | 30 [-] Show Material materials with Dureza Rockwell C of 30 [-] | |
Elongación A5 | 23.0 °C | 10 - 25 % Show Material materials with Elongación A5 of 10 - 25 % | |
Estricción | 23.0 °C | 6 - 25 % Show Material materials with Estricción of 6 - 25 % | |
Límite elástico | 23.0 °C | 580 - 880 MPa Show Material materials with Límite elástico of 580 - 880 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 23.0 °C | 205 GPa Show Material materials with Módulo elástico of 205 GPa | |
Resistencia a la tracción | 23.0 °C | 950 - 1190 MPa Show Material materials with Resistencia a la tracción of 950 - 1190 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.55E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.55E-5 1/K | The mentioned values are between 20°C and the mentioned temperature |
300.0 °C | 1.75E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.75E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
500.0 °C | 1.85E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.85E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
700.0 °C | 1.88E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.88E-5 1/K | The mentioned values are between 20°C and the mentioned temperature | |
Conductividad térmica | 23.0 °C | 14.5 W/(m·K) Show Material materials with Conductividad térmica of 14.5 W/(m·K) | |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 8.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % | |
Carbono | 0.45 - 0.55 % Show Material materials with Carbono of 0.45 - 0.55 % | |
Cromo | 20 - 22 % Show Material materials with Cromo of 20 - 22 % | |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % | |
Hierro | 59.4 - 66.85 % Show Material materials with Hierro of 59.4 - 66.85 % | Balance |
Manganeso | 8 - 10 % Show Material materials with Manganeso of 8 - 10 % | |
Nitrógeno | 0.4 - 0.6 % Show Material materials with Nitrógeno of 0.4 - 0.6 % | |
Níquel | 3.5 - 5.5 % Show Material materials with Níquel of 3.5 - 5.5 % | |
Silicona | 0.45 % Show Material materials with Silicona of 0.45 % | |
Wolframio | 0.8 - 1.5 % Show Material materials with Wolframio of 0.8 - 1.5 % |