General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 8.13 g/cm³ Show Material materials with Densidad of 8.13 g/cm³ |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 760.0 °C | 1.53E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.53E-5 1/K | The mentioned value is between 20°C and the mentioned temperature |
Chemical properties
Property | Value |
---|---|
Aluminio | 1 % Show Material materials with Aluminio of 1 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cromo | 27.8 % Show Material materials with Cromo of 27.8 % |
Hierro | 60.2 - 100 % Show Material materials with Hierro of 60.2 - 100 % |
Manganeso | 8.5 % Show Material materials with Manganeso of 8.5 % |
Níquel | 0.4 % Show Material materials with Níquel of 0.4 % |