Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Rockwell C | 23.0 °C | 32 - 45 [-] Show Material materials with Dureza Rockwell C of 32 - 45 [-] |
Estricción | 23.0 °C | 15 % Show Material materials with Estricción of 15 % |
Límite elástico | 23.0 °C | 1030 MPa Show Material materials with Límite elástico of 1030 MPa |
Resistencia a la tracción | 23.0 °C | 1280 MPa Show Material materials with Resistencia a la tracción of 1280 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 1.2 - 1.6 % Show Material materials with Aluminio of 1.2 - 1.6 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Boro | 0.003 - 0.01 % Show Material materials with Boro of 0.003 - 0.01 % |
Carbono | 0.03 - 0.1 % Show Material materials with Carbono of 0.03 - 0.1 % |
Circonio | 0.02 - 0.12 % Show Material materials with Circonio of 0.02 - 0.12 % |
Cobalto | 12 - 15 % Show Material materials with Cobalto of 12 - 15 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Cromo | 18 - 21 % Show Material materials with Cromo of 18 - 21 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 3.5 - 5 % Show Material materials with Molibdeno of 3.5 - 5 % |
Silicona | 0.75 % Show Material materials with Silicona of 0.75 % |
Titanio | 2.75 - 3.5 % Show Material materials with Titanio of 2.75 - 3.5 % |