Mecánica
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Boro | 0.05 % Show Material materials with Boro of 0.05 % |
Carbono | 0.04 % Show Material materials with Carbono of 0.04 % |
Cromo | 19 % Show Material materials with Cromo of 19 % |
Hierro | 21.21 - 100 % Show Material materials with Hierro of 21.21 - 100 % |
Manganeso | 0.2 % Show Material materials with Manganeso of 0.2 % |
Níquel | 52.5 % Show Material materials with Níquel of 52.5 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |