General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Austenitic Stainless Steel |
Elongación | 20.0 °C | 2 % Show Material materials with Elongación of 2 % | |
Elongación A80 | 20.0 °C | 2 % Show Material materials with Elongación A80 of 2 % | |
Límite elástico Rp 0,2 | 20.0 °C | 1380 MPa Show Material materials with Límite elástico Rp 0,2 of 1380 MPa | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Austenitic Stainless Steel |
Módulo elástico | 20.0 °C | 200 GPa Show Material materials with Módulo elástico of 200 GPa | |
100.0 °C | 195 GPa Show Material materials with Módulo elástico of 195 GPa | ||
200.0 °C | 185 GPa Show Material materials with Módulo elástico of 185 GPa | ||
300.0 °C | 175 GPa Show Material materials with Módulo elástico of 175 GPa | ||
400.0 °C | 170 GPa Show Material materials with Módulo elástico of 170 GPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 500 J/(kg·K) Show Material materials with Calor específico of 500 J/(kg·K) | |
Coeficiente de dilatación térmica | 100.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | |
300.0 °C | 1.44E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.44E-5 1/K | ||
Conductividad térmica | 20.0 °C | 16 W/(m·K) Show Material materials with Conductividad térmica of 16 W/(m·K) | |
Temperatura de fusión | 1230 - 1480 °C Show Material materials with Temperatura de fusión of 1230 - 1480 °C | Typical for Austenitic Stainless Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 8E-7 Ω·m Show Material materials with Resistividad eléctrica of 8E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.7 - 1.5 % Show Material materials with Aluminio of 0.7 - 1.5 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cromo | 14 - 16 % Show Material materials with Cromo of 14 - 16 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 1.2 % Show Material materials with Manganeso of 1.2 % |
Molibdeno | 2 - 3 % Show Material materials with Molibdeno of 2 - 3 % |
Níquel | 6.5 - 7.8 % Show Material materials with Níquel of 6.5 - 7.8 % |
Silicona | 0.7 % Show Material materials with Silicona of 0.7 % |