Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Molybdenum Steel |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Molybdenum Steel | ||||
Dureza Brinell | 242 [-] Show Material materials with Dureza Brinell of 242 [-] | Predicted Value, Transverse | ||||
Elongación | 15.9 % Show Material materials with Elongación of 15.9 % | Predicted Value, A200 | ||||
16.0 % Show Material materials with Elongación of 16.0 % | Predicted Value, A80 | |||||
18.4 % Show Material materials with Elongación of 18.4 % | Predicted Value, A80 Transverse | |||||
19.5 % Show Material materials with Elongación of 19.5 % | Predicted Value, A5 | |||||
20.6 % Show Material materials with Elongación of 20.6 % | Predicted Value, A50 | |||||
20 °C | 20 % Show Material materials with Elongación of 20 % | quenched and tempered (+QT) | EN 10028-2 | Flat | Transverse | |
20 °C | 20 % Show Material materials with Elongación of 20 % | quenched and tempered (+QT) | EN 10028-2 | Flat | ||
Estricción | 43.0 % Show Material materials with Estricción of 43.0 % | Predicted Value | ||||
44.8 % Show Material materials with Estricción of 44.8 % | Predicted Value, Transverse | |||||
Módulo de cizallamiento | 79.5 GPa Show Material materials with Módulo de cizallamiento of 79.5 GPa | Predicted Value | ||||
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Molybdenum Steel | ||||
Resistencia a la tracción | 20 °C | 480 - 620 MPa Show Material materials with Resistencia a la tracción of 480 - 620 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | Transverse |
20 °C | 480 - 620 MPa Show Material materials with Resistencia a la tracción of 480 - 620 MPa | quenched and tempered (+QT) | EN 10028-2 | Flat | ||
Resistencia al cizallamiento | 691.1 MPa Show Material materials with Resistencia al cizallamiento of 691.1 MPa | Predicted Value |
Aplicaciones térmicas
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Calor específico | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Molybdenum Steel | |||
Coeficiente de dilatación térmica | 1.29e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.29e-05 1/K | Typical for Molybdenum Steel | |||
Conductividad térmica | 37 - 48 W/(m·K) Show Material materials with Conductividad térmica of 37 - 48 W/(m·K) | Typical for Molybdenum Steel | |||
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Molybdenum Steel | |||
Temperatura máx. de funcionamiento | 20 - 450 °C Show Material materials with Temperatura máx. de funcionamiento of 20 - 450 °C | quenched and tempered (+QT) | EN 10028-2 | Flat | Long |
450 °C Show Material materials with Temperatura máx. de funcionamiento of 450 °C | quenched and tempered (+QT) | EN 10028-2 | Flat | Long |
Eléctrico
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.005 % Show Material materials with Azufre of 0.005 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
0.01 % Show Material materials with Azufre of 0.01 % | quenched and tempered (+QT) | EN 10028-2 | Flat | |
Carbono | 0.2 % Show Material materials with Carbono of 0.2 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Cobre | 0.3 % Show Material materials with Cobre of 0.3 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Cromo | 0.3 % Show Material materials with Cromo of 0.3 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Fósforo | 0.015 % Show Material materials with Fósforo of 0.015 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Manganeso | 0.9 - 1.5 % Show Material materials with Manganeso of 0.9 - 1.5 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Molibdeno | 0.45 - 0.6 % Show Material materials with Molibdeno of 0.45 - 0.6 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Nitrógeno | 0.012 % Show Material materials with Nitrógeno of 0.012 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Níquel | 0.3 % Show Material materials with Níquel of 0.3 % | quenched and tempered (+QT) | EN 10028-2 | Flat |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % | quenched and tempered (+QT) | EN 10028-2 | Flat |