General
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Densidad | 20 °C | 7.86 g/cm³ Show Material materials with Densidad of 7.86 g/cm³ | quenched and tempered (+QT) | EN 10028-4 | Flat |
27 °C | 7.821 g/cm³ Show Material materials with Densidad of 7.821 g/cm³ | quenched and tempered (+QT) | EN 10028-4 | Flat |
Mecánica
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Coeficiente de Poisson | -269 °C | 0.281 [-] Show Material materials with Coeficiente de Poisson of 0.281 [-] | quenched and tempered (+QT) | EN 10028-4 | Flat | |
-200 °C | 0.281 [-] Show Material materials with Coeficiente de Poisson of 0.281 [-] | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-150 °C | 0.282 [-] Show Material materials with Coeficiente de Poisson of 0.282 [-] | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-100 °C | 0.283 [-] Show Material materials with Coeficiente de Poisson of 0.283 [-] | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-50 °C | 0.285 [-] Show Material materials with Coeficiente de Poisson of 0.285 [-] | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
27 °C | 0.288 [-] Show Material materials with Coeficiente de Poisson of 0.288 [-] | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Dureza Brinell | 250 [-] Show Material materials with Dureza Brinell of 250 [-] | Predicted Value, Transverse | ||||
Elongación | 16.1 % Show Material materials with Elongación of 16.1 % | Predicted Value, A200 | ||||
20.5 % Show Material materials with Elongación of 20.5 % | Predicted Value, Transverse | |||||
21.1 % Show Material materials with Elongación of 21.1 % | Predicted Value, A50 | |||||
21.5 % Show Material materials with Elongación of 21.5 % | Predicted Value, A80 | |||||
21.9 % Show Material materials with Elongación of 21.9 % | Predicted Value, A5 | |||||
25.4 % Show Material materials with Elongación of 25.4 % | Predicted Value, A80 Transverse | |||||
20 °C | 20 % Show Material materials with Elongación of 20 % | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Estricción | 42.4 % Show Material materials with Estricción of 42.4 % | Predicted Value | ||||
42.6 % Show Material materials with Estricción of 42.6 % | Predicted Value, Transverse | |||||
Límite elástico | 254.9 MPa Show Material materials with Límite elástico of 254.9 MPa | Predicted Value, RP1 | ||||
313.3 MPa Show Material materials with Límite elástico of 313.3 MPa | Predicted Value, RP1 Transverse | |||||
353.8 MPa Show Material materials with Límite elástico of 353.8 MPa | Predicted Value, Transverse | |||||
371.5 MPa Show Material materials with Límite elástico of 371.5 MPa | Predicted Value, RP05 | |||||
424.4 MPa Show Material materials with Límite elástico of 424.4 MPa | Predicted Value, RP02 | |||||
446.4 MPa Show Material materials with Límite elástico of 446.4 MPa | Predicted Value, RP02 Transverse | |||||
510.7 MPa Show Material materials with Límite elástico of 510.7 MPa | Predicted Value, RP002 | |||||
20 °C | 380 MPa Show Material materials with Límite elástico of 380 MPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
20 °C | 390 MPa Show Material materials with Límite elástico of 390 MPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Módulo de cizallamiento | -269 °C | 81.7 GPa Show Material materials with Módulo de cizallamiento of 81.7 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | |
-200 °C | 81.8 GPa Show Material materials with Módulo de cizallamiento of 81.8 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-150 °C | 81.1 GPa Show Material materials with Módulo de cizallamiento of 81.1 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-100 °C | 80.2 GPa Show Material materials with Módulo de cizallamiento of 80.2 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-50 °C | 79 GPa Show Material materials with Módulo de cizallamiento of 79 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
27 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Módulo elástico | -269 °C | 209.4 GPa Show Material materials with Módulo elástico of 209.4 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | |
-200 °C | 209.5 GPa Show Material materials with Módulo elástico of 209.5 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-150 °C | 208 GPa Show Material materials with Módulo elástico of 208 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-100 °C | 205.9 - 210 GPa Show Material materials with Módulo elástico of 205.9 - 210 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-100 °C | 205.9 GPa Show Material materials with Módulo elástico of 205.9 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-100 °C | 210 GPa Show Material materials with Módulo elástico of 210 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
-50 °C | 203.1 GPa Show Material materials with Módulo elástico of 203.1 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
20 °C | 204 GPa Show Material materials with Módulo elástico of 204 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
27 °C | 198.4 GPa Show Material materials with Módulo elástico of 198.4 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
100 °C | 199 GPa Show Material materials with Módulo elástico of 199 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
200 °C | 193 GPa Show Material materials with Módulo elástico of 193 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
300 °C | 186 GPa Show Material materials with Módulo elástico of 186 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
400 °C | 178 GPa Show Material materials with Módulo elástico of 178 GPa | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Resistencia a la tracción | 20 °C | 530 - 710 MPa Show Material materials with Resistencia a la tracción of 530 - 710 MPa | quenched and tempered (+QT) | EN 10028-4 | Flat | |
Resistencia al cizallamiento | 526.3 MPa Show Material materials with Resistencia al cizallamiento of 526.3 MPa | Predicted Value |
Aplicaciones térmicas
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Calor específico | -100 °C | 440 J/(kg·K) Show Material materials with Calor específico of 440 J/(kg·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | |
20 °C | 463 J/(kg·K) Show Material materials with Calor específico of 463 J/(kg·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
100 °C | 477 J/(kg·K) Show Material materials with Calor específico of 477 J/(kg·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
200 °C | 494 J/(kg·K) Show Material materials with Calor específico of 494 J/(kg·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
300 °C | 510 J/(kg·K) Show Material materials with Calor específico of 510 J/(kg·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
400 °C | 529 J/(kg·K) Show Material materials with Calor específico of 529 J/(kg·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Coeficiente de dilatación térmica | -100 °C | 1.02e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.02e-05 1/K | quenched and tempered (+QT) | EN 10028-4 | Flat | |
20 °C | 1.12e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.12e-05 1/K | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
100 °C | 1.17e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.17e-05 1/K | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
200 °C | 1.21e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.21e-05 1/K | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
300 °C | 1.25e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.25e-05 1/K | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
400 °C | 1.28e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.28e-05 1/K | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Conductividad térmica | -100 °C | 29.5 W/(m·K) Show Material materials with Conductividad térmica of 29.5 W/(m·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | |
20 °C | 36.2 W/(m·K) Show Material materials with Conductividad térmica of 36.2 W/(m·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
100 °C | 38.5 W/(m·K) Show Material materials with Conductividad térmica of 38.5 W/(m·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
200 °C | 39 W/(m·K) Show Material materials with Conductividad térmica of 39 W/(m·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
300 °C | 38.3 W/(m·K) Show Material materials with Conductividad térmica of 38.3 W/(m·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
400 °C | 36.2 W/(m·K) Show Material materials with Conductividad térmica of 36.2 W/(m·K) | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Difusividad térmica | 20 °C | 10 mm²/s Show Material materials with Difusividad térmica of 10 mm²/s | quenched and tempered (+QT) | EN 10028-4 | Flat | |
100 °C | 10 mm²/s Show Material materials with Difusividad térmica of 10 mm²/s | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
200 °C | 9.6 mm²/s Show Material materials with Difusividad térmica of 9.6 mm²/s | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
300 °C | 8.8 mm²/s Show Material materials with Difusividad térmica of 8.8 mm²/s | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
400 °C | 7.7 mm²/s Show Material materials with Difusividad térmica of 7.7 mm²/s | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel | ||||
Temperatura máx. de funcionamiento | -150 °C Show Material materials with Temperatura máx. de funcionamiento of -150 °C | quenched and tempered (+QT) | EN 10028-4 | Flat | Long | |
-120 °C Show Material materials with Temperatura máx. de funcionamiento of -120 °C | quenched and tempered (+QT) | EN 10028-4 | Flat | Long |
Eléctrico
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Conductividad eléctrica | 6 S/m Show Material materials with Conductividad eléctrica of 6 S/m | Predicted Value | ||||
Resistividad eléctrica | -100 °C | 1.95e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.95e-07 Ω·m | quenched and tempered (+QT) | EN 10028-4 | Flat | |
20 °C | 2.61e-07 Ω·m Show Material materials with Resistividad eléctrica of 2.61e-07 Ω·m | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
100 °C | 3.1e-07 Ω·m Show Material materials with Resistividad eléctrica of 3.1e-07 Ω·m | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
200 °C | 3.78e-07 Ω·m Show Material materials with Resistividad eléctrica of 3.78e-07 Ω·m | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
300 °C | 4.57e-07 Ω·m Show Material materials with Resistividad eléctrica of 4.57e-07 Ω·m | quenched and tempered (+QT) | EN 10028-4 | Flat | ||
400 °C | 5.57e-07 Ω·m Show Material materials with Resistividad eléctrica of 5.57e-07 Ω·m | quenched and tempered (+QT) | EN 10028-4 | Flat |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Azufre | 0.005 % Show Material materials with Azufre of 0.005 % | quenched and tempered (+QT) | EN 10028-4 | Flat |
0.01 % Show Material materials with Azufre of 0.01 % | quenched and tempered (+QT) | EN 10028-4 | Flat | |
Carbono | 0.15 % Show Material materials with Carbono of 0.15 % | quenched and tempered (+QT) | EN 10028-4 | Flat |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % | quenched and tempered (+QT) | EN 10028-4 | Flat |
Manganeso | 0.3 - 0.8 % Show Material materials with Manganeso of 0.3 - 0.8 % | quenched and tempered (+QT) | EN 10028-4 | Flat |
Níquel | 4.75 - 5.25 % Show Material materials with Níquel of 4.75 - 5.25 % | quenched and tempered (+QT) | EN 10028-4 | Flat |
Silicona | 0.35 % Show Material materials with Silicona of 0.35 % | quenched and tempered (+QT) | EN 10028-4 | Flat |
Vanadio | 0.05 % Show Material materials with Vanadio of 0.05 % | quenched and tempered (+QT) | EN 10028-4 | Flat |
Technological properties
Property | ||
---|---|---|