Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 137 - 197 [-] Show Material materials with Dureza Brinell of 137 - 197 [-] |
Elongación A50 | 20.0 °C | 18 % Show Material materials with Elongación A50 of 18 % |
Estricción | 20.0 °C | 33 % Show Material materials with Estricción of 33 % |
Resistencia a la tracción | 20.0 °C | 485 - 655 MPa Show Material materials with Resistencia a la tracción of 485 - 655 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 250 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 250 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.3 % Show Material materials with Carbono of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 1.05 % Show Material materials with Manganeso of 0.4 - 1.05 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |