Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 23.0 °C | 25 % Show Material materials with Elongación A50 of 25 % |
Elongation A200 | 23.0 °C | 22 % Show Material materials with Elongation A200 of 22 % |
Límite elástico | 23.0 °C | 205 MPa Show Material materials with Límite elástico of 205 MPa |
Resistencia a la tracción | 23.0 °C | 380 - 515 MPa Show Material materials with Resistencia a la tracción of 380 - 515 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.24 % Show Material materials with Carbono of 0.24 % |
Cobre | 0.2 % Show Material materials with Cobre of 0.2 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.9 % Show Material materials with Manganeso of 0.9 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |