Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 217 [-] Show Material materials with Dureza Brinell of 217 [-] |
Elongación A50 | 20.0 °C | 18 % Show Material materials with Elongación A50 of 18 % |
Resistencia a la tracción | 20.0 °C | 725 - 895 MPa Show Material materials with Resistencia a la tracción of 725 - 895 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 585 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 585 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.23 % Show Material materials with Carbono of 0.23 % |
Cromo | 1.5 - 2 % Show Material materials with Cromo of 1.5 - 2 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Manganeso | 0.2 - 0.4 % Show Material materials with Manganeso of 0.2 - 0.4 % |
Molibdeno | 0.4 - 0.6 % Show Material materials with Molibdeno of 0.4 - 0.6 % |
Níquel | 2.8 - 3.9 % Show Material materials with Níquel of 2.8 - 3.9 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Vanadio | 0.08 % Show Material materials with Vanadio of 0.08 % |