Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 121 - 170 [-] Show Material materials with Dureza Brinell of 121 - 170 [-] |
Elongación A50 | 20.0 °C | 21 % Show Material materials with Elongación A50 of 21 % |
Estricción | 20.0 °C | 38 % Show Material materials with Estricción of 38 % |
Resistencia a la tracción | 20.0 °C | 415 - 585 MPa Show Material materials with Resistencia a la tracción of 415 - 585 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 205 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 205 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.3 % Show Material materials with Carbono of 0.3 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.4 - 1.05 % Show Material materials with Manganeso of 0.4 - 1.05 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |