General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 20.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 20.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Low Carbon Steel |
Dureza Vickers | 20.0 °C | 105 - 115 [-] Show Material materials with Dureza Vickers of 105 - 115 [-] | |
Elongación | 20.0 °C | 40 % Show Material materials with Elongación of 40 % | |
Elongación A50 | 20.0 °C | 32 - 40 % Show Material materials with Elongación A50 of 32 - 40 % | |
Elongación A80 | 20.0 °C | 30 - 38 % Show Material materials with Elongación A80 of 30 - 38 % | |
Límite elástico | 20.0 °C | 140 - 250 MPa Show Material materials with Límite elástico of 140 - 250 MPa | |
Módulo elástico | 20.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Low Carbon Steel |
Resistencia a la tracción | 20.0 °C | 35 - 350 MPa Show Material materials with Resistencia a la tracción of 35 - 350 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 20.0 °C | 1.32E-5 - 1.38E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | Typical for Low Carbon Steel |
Magnético
Property | Value | Comment |
---|---|---|
Temperatura de Curie | 770 °C Show Material materials with Temperatura de Curie of 770 °C | Typical for Low Carbon Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 - 0.035 % Show Material materials with Azufre of 0.03 - 0.035 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Fósforo | 0.03 - 0.04 % Show Material materials with Fósforo of 0.03 - 0.04 % |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % |