General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 3.2 g/cm³ Show Material materials with Densidad of 3.2 g/cm³ | Typical for Ferrosilicon |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 1250 GPa Show Material materials with Módulo elástico of 1250 GPa | Typical for Ferrosilicon |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 1200 °C Show Material materials with Temperatura de fusión of 1200 °C | Typical for Ferrosilicon |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Fósforo | 0.04 % Show Material materials with Fósforo of 0.04 % |
Manganeso | 0.4 % Show Material materials with Manganeso of 0.4 % |
Silicona | 74 - 79 % Show Material materials with Silicona of 74 - 79 % |