General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Cast Copper Nickel Grade |
Dureza Brinell | 20.0 °C | 115 [-] Show Material materials with Dureza Brinell of 115 [-] | |
Elongación | 20.0 °C | 18 % Show Material materials with Elongación of 18 % | |
Límite elástico Rp 0,2 | 20.0 °C | 150 MPa Show Material materials with Límite elástico Rp 0,2 of 150 MPa | |
Módulo elástico | 20.0 °C | 145 GPa Show Material materials with Módulo elástico of 145 GPa | |
Resistencia a la tracción | 20.0 °C | 440 MPa Show Material materials with Resistencia a la tracción of 440 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 J/(kg·K) Show Material materials with Calor específico of 377 J/(kg·K) | Typical for Cast Copper Nickel Grade |
Coeficiente de dilatación térmica | 300.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | |
Conductividad térmica | 20.0 °C | 29 W/(m·K) Show Material materials with Conductividad térmica of 29 W/(m·K) | |
Temperatura de fusión | 1100 - 1240 °C Show Material materials with Temperatura de fusión of 1100 - 1240 °C | Typical for Cast Copper Nickel Grade |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.50E+6 S/m Show Material materials with Conductividad eléctrica of 2.50E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Bismuto | 0.01 % Show Material materials with Bismuto of 0.01 % |
Boro | 0.01 % Show Material materials with Boro of 0.01 % |
Cadmio | 0.02 % Show Material materials with Cadmio of 0.02 % |
Carbono | 0.03 % Show Material materials with Carbono of 0.03 % |
Cobre | 64 % Show Material materials with Cobre of 64 % |
Fósforo | 0.01 % Show Material materials with Fósforo of 0.01 % |
Hierro | 0.5 - 1.5 % Show Material materials with Hierro of 0.5 - 1.5 % |
Magnesio | 0.01 % Show Material materials with Magnesio of 0.01 % |
Manganeso | 0.6 - 1.2 % Show Material materials with Manganeso of 0.6 - 1.2 % |
Niobio | 0.5 - 1 % Show Material materials with Niobio of 0.5 - 1 % |
Níquel | 29 - 31 % Show Material materials with Níquel of 29 - 31 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Selenio | 0.01 % Show Material materials with Selenio of 0.01 % |
Silicona | 0.3 - 0.7 % Show Material materials with Silicona of 0.3 - 0.7 % |
Telurio | 0.01 % Show Material materials with Telurio of 0.01 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting, separately cast test sample |