General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 1.74 g/cm³ Show Material materials with Densidad of 1.74 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Magnesium |
Dureza Brinell | 20.0 °C | 38 [-] Show Material materials with Dureza Brinell of 38 [-] | |
Módulo de cizallamiento | 23.0 °C | 45 GPa Show Material materials with Módulo de cizallamiento of 45 GPa | Typical for Magnesium |
Módulo elástico | 20.0 °C | 45 GPa Show Material materials with Módulo elástico of 45 GPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 1010 - 1060 J/(kg·K) Show Material materials with Calor específico of 1010 - 1060 J/(kg·K) | Typical for Magnesium |
Coeficiente de dilatación térmica | 23.0 °C | 1.3E-5 - 2.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 - 2.6E-5 1/K | Typical for Magnesium |
Conductividad térmica | 20.0 °C | 155 W/(m·K) Show Material materials with Conductividad térmica of 155 W/(m·K) | |
Temperatura de fusión | 650 °C Show Material materials with Temperatura de fusión of 650 °C | Typical for Magnesium |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 2.24E+7 S/m Show Material materials with Conductividad eléctrica of 2.24E+7 S/m |
Chemical properties
Property | Value |
---|---|
Cobre | 0.02 % Show Material materials with Cobre of 0.02 % |
Hierro | 0.05 % Show Material materials with Hierro of 0.05 % |
Magnesio | 99.8 % Show Material materials with Magnesio of 99.8 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 2E-3 % Show Material materials with Níquel of 2E-3 % |
Silicona | 0.1 % Show Material materials with Silicona of 0.1 % |