General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.75 g/cm³ Show Material materials with Densidad of 7.75 g/cm³ | Typical for Iron Alloy |
Mecánica
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de dilatación térmica | 23.0 °C | 1E-5 - 2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1E-5 - 2E-5 1/K | Typical for Iron Alloy |
Chemical properties
Technological properties
Property | ||
---|---|---|
Features | Soft magnetic |