General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 150 [-] Show Material materials with Dureza Brinell of 150 [-] |
Elongación | 20.0 °C | 15 - 20 % Show Material materials with Elongación of 15 - 20 % |
Elongation A100 | 20.0 °C | 5 - 10 % Show Material materials with Elongation A100 of 5 - 10 % |
Límite elástico Rp 0,2 | 20.0 °C | 290 - 340 MPa Show Material materials with Límite elástico Rp 0,2 of 290 - 340 MPa |
Módulo elástico | 20.0 °C | 208 GPa Show Material materials with Módulo elástico of 208 GPa |
Resistencia a la tracción | 20.0 °C | 490 - 550 MPa Show Material materials with Resistencia a la tracción of 490 - 550 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | |
Coeficiente de dilatación térmica | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Conductividad térmica | 20.0 °C | 79 W/(m·K) Show Material materials with Conductividad térmica of 79 W/(m·K) | |
Temperatura de fusión | 1400 - 1500 °C Show Material materials with Temperatura de fusión of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 9.5E-8 Ω·m Show Material materials with Resistividad eléctrica of 9.5E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Carbono | 0.08 % Show Material materials with Carbono of 0.08 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % |
Hierro | 0.25 % Show Material materials with Hierro of 0.25 % |
Magnesio | 0.15 % Show Material materials with Magnesio of 0.15 % |
Manganeso | 0.35 % Show Material materials with Manganeso of 0.35 % |
Níquel | 98.6 % Show Material materials with Níquel of 98.6 % |
Silicona | 0.15 % Show Material materials with Silicona of 0.15 % |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % |