General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.46 g/cm³ Show Material materials with Densidad of 8.46 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 265 [-] Show Material materials with Dureza Brinell of 265 [-] |
Elongación | -80.0 °C | 18 % Show Material materials with Elongación of 18 % |
20.0 °C | 17 - 23 % Show Material materials with Elongación of 17 - 23 % | |
100.0 °C | 23 % Show Material materials with Elongación of 23 % | |
200.0 °C | 23 % Show Material materials with Elongación of 23 % | |
300.0 °C | 23 % Show Material materials with Elongación of 23 % | |
400.0 °C | 12 % Show Material materials with Elongación of 12 % | |
500.0 °C | 4.5 % Show Material materials with Elongación of 4.5 % | |
600.0 °C | 1.5 % Show Material materials with Elongación of 1.5 % | |
700.0 °C | 3.5 % Show Material materials with Elongación of 3.5 % | |
Límite elástico Rp 0,2 | -80.0 °C | 785 MPa Show Material materials with Límite elástico Rp 0,2 of 785 MPa |
20.0 °C | 687 - 755 MPa Show Material materials with Límite elástico Rp 0,2 of 687 - 755 MPa | |
100.0 °C | 736 MPa Show Material materials with Límite elástico Rp 0,2 of 736 MPa | |
200.0 °C | 716 MPa Show Material materials with Límite elástico Rp 0,2 of 716 MPa | |
300.0 °C | 716 MPa Show Material materials with Límite elástico Rp 0,2 of 716 MPa | |
400.0 °C | 716 MPa Show Material materials with Límite elástico Rp 0,2 of 716 MPa | |
500.0 °C | 677 MPa Show Material materials with Límite elástico Rp 0,2 of 677 MPa | |
600.0 °C | 579 MPa Show Material materials with Límite elástico Rp 0,2 of 579 MPa | |
700.0 °C | 441 MPa Show Material materials with Límite elástico Rp 0,2 of 441 MPa | |
Módulo elástico | 20.0 °C | 178.54 GPa Show Material materials with Módulo elástico of 178.54 GPa |
100.0 °C | 174.62 GPa Show Material materials with Módulo elástico of 174.62 GPa | |
200.0 °C | 170.69 GPa Show Material materials with Módulo elástico of 170.69 GPa | |
300.0 °C | 165.79 GPa Show Material materials with Módulo elástico of 165.79 GPa | |
400.0 °C | 159.9 GPa Show Material materials with Módulo elástico of 159.9 GPa | |
500.0 °C | 153.04 GPa Show Material materials with Módulo elástico of 153.04 GPa | |
Resistencia a la tracción | -80.0 °C | 1177 MPa Show Material materials with Resistencia a la tracción of 1177 MPa |
20.0 °C | 962 - 1079 MPa Show Material materials with Resistencia a la tracción of 962 - 1079 MPa | |
100.0 °C | 1030 MPa Show Material materials with Resistencia a la tracción of 1030 MPa | |
200.0 °C | 1020 MPa Show Material materials with Resistencia a la tracción of 1020 MPa | |
300.0 °C | 1010 MPa Show Material materials with Resistencia a la tracción of 1010 MPa | |
400.0 °C | 903 MPa Show Material materials with Resistencia a la tracción of 903 MPa | |
500.0 °C | 726 MPa Show Material materials with Resistencia a la tracción of 726 MPa | |
600.0 °C | 589 MPa Show Material materials with Resistencia a la tracción of 589 MPa | |
700.0 °C | 461 MPa Show Material materials with Resistencia a la tracción of 461 MPa | |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 427 J/(kg·K) Show Material materials with Calor específico of 427 J/(kg·K) | |
100.0 °C | 427 J/(kg·K) Show Material materials with Calor específico of 427 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | |
300.0 °C | 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 1/K | ||
600.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | ||
Conductividad térmica | 20.0 °C | 18 W/(m·K) Show Material materials with Conductividad térmica of 18 W/(m·K) | |
100.0 °C | 18 W/(m·K) Show Material materials with Conductividad térmica of 18 W/(m·K) | ||
Temperatura de fusión | 1170 - 1365 °C Show Material materials with Temperatura de fusión of 1170 - 1365 °C | Typical for Nickel Copper Alloy | |
Temperatura máx. de funcionamiento, largo | 0 - 450 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 450 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Conductividad eléctrica | 20.0 °C | 1.72E+6 S/m Show Material materials with Conductividad eléctrica of 1.72E+6 S/m |
Resistividad eléctrica | 20.0 °C | 5.47E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.47E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 2 - 4 % Show Material materials with Aluminio of 2 - 4 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.25 % Show Material materials with Carbono of 0.25 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 27 - 34 % Show Material materials with Cobre of 27 - 34 % |
Hierro | 2 % Show Material materials with Hierro of 2 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
Titanio | 0.25 - 1 % Show Material materials with Titanio of 0.25 - 1 % |