Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.1 - 8.2 g/cm³ Show Material materials with Densidad of 8.1 - 8.2 g/cm³ | Typical for Nickel Iron Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.28 [-] Show Material materials with Coeficiente de Poisson of 0.28 [-] | Typical for Nickel Iron Alloy |
Módulo elástico | 23.0 °C | 137 - 145 GPa Show Material materials with Módulo elástico of 137 - 145 GPa | Typical for Nickel Iron Alloy |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Iron Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 7.6E-6 - 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 7.6E-6 - 1.7E-5 1/K | Typical for Nickel Iron Alloy |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Iron Alloy |
Temperatura de fusión | 1450 °C Show Material materials with Temperatura de fusión of 1450 °C | Typical for Nickel Iron Alloy |
Chemical properties
Property | Value |
---|---|
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobre | 4 - 6 % Show Material materials with Cobre of 4 - 6 % |
Hierro | 12 - 16 % Show Material materials with Hierro of 12 - 16 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Molibdeno | 2 - 5 % Show Material materials with Molibdeno of 2 - 5 % |
Níquel | 71.55 % Show Material materials with Níquel of 71.55 % |
Silicona | 0.4 % Show Material materials with Silicona of 0.4 % |