Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ | Typical for Pure/Low Nickel Alloy |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 20.0 °C | 40 % Show Material materials with Elongación of 40 % | |
Elongation A100 | 20.0 °C | 20 - 30 % Show Material materials with Elongation A100 of 20 - 30 % | |
Módulo elástico | 23.0 °C | 190 - 220 GPa Show Material materials with Módulo elástico of 190 - 220 GPa | Typical for Pure/Low Nickel Alloy |
Resistencia a la tracción | 20.0 °C | 340 - 400 MPa Show Material materials with Resistencia a la tracción of 340 - 400 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Calor específico of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Conductividad térmica | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Conductividad térmica of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Temperatura de fusión | 1400 - 1500 °C Show Material materials with Temperatura de fusión of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy |
Chemical properties
Property | Value |
---|---|
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.15 - 0.25 % Show Material materials with Carbono of 0.15 - 0.25 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.5 % Show Material materials with Cobre of 0.5 % |
Hierro | 0.5 % Show Material materials with Hierro of 0.5 % |
Magnesio | 0.15 % Show Material materials with Magnesio of 0.15 % |
Manganeso | 0.7 - 1.3 % Show Material materials with Manganeso of 0.7 - 1.3 % |
Níquel | 97 % Show Material materials with Níquel of 97 % |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % |