Mecánica
Property | Temperature | Value |
---|---|---|
Elongación | 20.0 °C | 30 - 40 % Show Material materials with Elongación of 30 - 40 % |
Elongation A100 | 20.0 °C | 30 % Show Material materials with Elongation A100 of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 140 MPa Show Material materials with Límite elástico Rp 0,2 of 140 MPa |
Límite elástico Rp 1,0 | 20.0 °C | 170 MPa Show Material materials with Límite elástico Rp 1,0 of 170 MPa |
Resistencia a la tracción | 20.0 °C | 400 - 420 MPa Show Material materials with Resistencia a la tracción of 400 - 420 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 5E-3 % Show Material materials with Azufre of 5E-3 % |
Carbono | 0.05 % Show Material materials with Carbono of 0.05 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % |
Cromo | 1.4 - 1.8 % Show Material materials with Cromo of 1.4 - 1.8 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 1.3 - 1.8 % Show Material materials with Manganeso of 1.3 - 1.8 % |
Níquel | 94.5 % Show Material materials with Níquel of 94.5 % |
Silicona | 0.4 - 0.65 % Show Material materials with Silicona of 0.4 - 0.65 % |
Titanio | 0.1 % Show Material materials with Titanio of 0.1 % |