General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.9 g/cm³ Show Material materials with Densidad of 7.9 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 220 [-] Show Material materials with Dureza Brinell of 220 [-] |
Elongación | 20.0 °C | 30 % Show Material materials with Elongación of 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 270 MPa Show Material materials with Límite elástico Rp 0,2 of 270 MPa |
Límite elástico Rp 1,0 | 20.0 °C | 330 MPa Show Material materials with Límite elástico Rp 1,0 of 330 MPa |
Módulo elástico | 20.0 °C | 214 GPa Show Material materials with Módulo elástico of 214 GPa |
Resistencia a la tracción | 20.0 °C | 680 MPa Show Material materials with Resistencia a la tracción of 680 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 285 - 545 J/(kg·K) Show Material materials with Calor específico of 285 - 545 J/(kg·K) | Typical for Nickel Chromium Iron Alloy |
Coeficiente de dilatación térmica | 400.0 °C | 1.43E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.43E-5 1/K | |
Conductividad térmica | 23.0 °C | 8 - 35 W/(m·K) Show Material materials with Conductividad térmica of 8 - 35 W/(m·K) | Typical for Nickel Chromium Iron Alloy |
Temperatura de fusión | 1200 - 1480 °C Show Material materials with Temperatura de fusión of 1200 - 1480 °C | Typical for Nickel Chromium Iron Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.25E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.25E-6 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminio | 2.4 - 3 % Show Material materials with Aluminio of 2.4 - 3 % |
Azufre | 0.015 % Show Material materials with Azufre of 0.015 % |
Carbono | 0.2 - 0.4 % Show Material materials with Carbono of 0.2 - 0.4 % |
Circonio | 0.01 - 0.1 % Show Material materials with Circonio of 0.01 - 0.1 % |
Cobre | 0.15 % Show Material materials with Cobre of 0.15 % |
Cromo | 24 - 26 % Show Material materials with Cromo of 24 - 26 % |
Fósforo | 0.02 % Show Material materials with Fósforo of 0.02 % |
Hierro | 8 - 11 % Show Material materials with Hierro of 8 - 11 % |
Itrio | 0.05 - 0.15 % Show Material materials with Itrio of 0.05 - 0.15 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 58.3 % Show Material materials with Níquel of 58.3 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |
Titanio | 0.1 - 0.25 % Show Material materials with Titanio of 0.1 - 0.25 % |