General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.28 g/cm³ Show Material materials with Densidad of 7.28 g/cm³ | Typical for Pure/Low Alloyed Tin |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 205 - 238 J/(kg·K) Show Material materials with Calor específico of 205 - 238 J/(kg·K) | Typical for Pure/Low Alloyed Tin |
Coeficiente de dilatación térmica | 23.0 °C | 2.1E-5 - 2.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2.1E-5 - 2.9E-5 1/K | Typical for Pure/Low Alloyed Tin |
Conductividad térmica | 23.0 °C | 52 - 74 W/(m·K) Show Material materials with Conductividad térmica of 52 - 74 W/(m·K) | Typical for Pure/Low Alloyed Tin |
Temperatura de fusión | 232 °C Show Material materials with Temperatura de fusión of 232 °C | Typical for Pure/Low Alloyed Tin |
Chemical properties
Property | Value |
---|---|
Estaño | 99.5 % Show Material materials with Estaño of 99.5 % |