Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Temperatura de fusión | 1480 °C Show Material materials with Temperatura de fusión of 1480 °C | Typical for Ferrovanadium |
Chemical properties
Property | Value |
---|---|
Aluminio | 2 % Show Material materials with Aluminio of 2 % |
Azufre | 0.08 % Show Material materials with Azufre of 0.08 % |
Carbono | 0.75 % Show Material materials with Carbono of 0.75 % |
Fósforo | 0.08 % Show Material materials with Fósforo of 0.08 % |
Silicona | 1.5 % Show Material materials with Silicona of 1.5 % |
Vanadio | 75 - 85 % Show Material materials with Vanadio of 75 - 85 % |