General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 9.6 g/cm³ Show Material materials with Densidad of 9.6 g/cm³ | Typical for Lead Antimony |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Calor específico of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Conductividad térmica | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Conductividad térmica of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Temperatura de fusión | 235 - 305 °C Show Material materials with Temperatura de fusión of 235 - 305 °C | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.01 % Show Material materials with Aluminio of 0.01 % |
Antimonio | 14 - 15.5 % Show Material materials with Antimonio of 14 - 15.5 % |
Arsénico | 0.75 - 1.25 % Show Material materials with Arsénico of 0.75 - 1.25 % |
Cobre | 0.1 - 0.5 % Show Material materials with Cobre of 0.1 - 0.5 % |
Estaño | 0.8 - 1.2 % Show Material materials with Estaño of 0.8 - 1.2 % |
Hierro | 0.1 % Show Material materials with Hierro of 0.1 % |
Plomo | 81.38 % Show Material materials with Plomo of 81.38 % |
Zinc | 0.05 % Show Material materials with Zinc of 0.05 % |