Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 213 - 239 J/(kg·K) Show Material materials with Calor específico of 213 - 239 J/(kg·K) | Typical for Lead Tin |
Conductividad térmica | 23.0 °C | 35 - 57 W/(m·K) Show Material materials with Conductividad térmica of 35 - 57 W/(m·K) | Typical for Lead Tin |
Temperatura de fusión | 185 - 320 °C Show Material materials with Temperatura de fusión of 185 - 320 °C | Typical for Lead Tin |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % | |
Antimonio | 2.75 % Show Material materials with Antimonio of 2.75 % | |
Bismuto | 0.25 % Show Material materials with Bismuto of 0.25 % | |
Cobre | 0.08 % Show Material materials with Cobre of 0.08 % | In dipping solders, 0.5% max copper is permissible |
Estaño | 14 - 15 % Show Material materials with Estaño of 14 - 15 % | |
Hierro | 0.02 % Show Material materials with Hierro of 0.02 % | |
Zinc | 5E-3 % Show Material materials with Zinc of 5E-3 % |