General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.12 - 0.18 % Show Material materials with Carbono of 0.12 - 0.18 % |
Cromo | 0.2 - 0.5 % Show Material materials with Cromo of 0.2 - 0.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Hierro | 95.76 - 97.18 % Show Material materials with Hierro of 95.76 - 97.18 % |
Manganeso | 0.35 - 0.65 % Show Material materials with Manganeso of 0.35 - 0.65 % |
Níquel | 2 - 2.5 % Show Material materials with Níquel of 2 - 2.5 % |
Silicona | 0.15 - 0.35 % Show Material materials with Silicona of 0.15 - 0.35 % |