Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
ASTM A132 Grade A1
Los datos sobre este material han sido proporcionados por ASTM.
All categories
Let us help you find the best supplier!
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value |
---|---|
Azufre | 0.15 % Show Material materials with Azufre of 0.15 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cobre | 1 % Show Material materials with Cobre of 1 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Molibdeno | 60 % Show Material materials with Molibdeno of 60 % |
Silicona | 1 % Show Material materials with Silicona of 1 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.