Chemical properties
Property | Value |
---|---|
Aluminio | 5E-3 % Show Material materials with Aluminio of 5E-3 % |
Antimonio | 0.8 % Show Material materials with Antimonio of 0.8 % |
Azufre | 0.08 % Show Material materials with Azufre of 0.08 % |
Cobre | 67 - 72 % Show Material materials with Cobre of 67 - 72 % |
Estaño | 4.5 - 6 % Show Material materials with Estaño of 4.5 - 6 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Hierro | 0.15 % Show Material materials with Hierro of 0.15 % |
Níquel | 1 % Show Material materials with Níquel of 1 % |
Plomo | 23 - 27 % Show Material materials with Plomo of 23 - 27 % |
Silicona | 5E-3 % Show Material materials with Silicona of 5E-3 % |
Zinc | 0.8 % Show Material materials with Zinc of 0.8 % |