General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.7 g/cm³ Show Material materials with Densidad of 7.7 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | Typical for Cast Iron |
Dureza Brinell | 20.0 °C | 430 - 690 [-] Show Material materials with Dureza Brinell of 430 - 690 [-] | |
Dureza Vickers | 20.0 °C | 450 - 750 [-] Show Material materials with Dureza Vickers of 450 - 750 [-] | |
Módulo de cizallamiento | 23.0 °C | 41 GPa Show Material materials with Módulo de cizallamiento of 41 GPa | Typical for Cast Iron |
Módulo elástico | 20.0 °C | 169 - 183 GPa Show Material materials with Módulo elástico of 169 - 183 GPa | |
Resistencia a la tracción | 20.0 °C | 320 - 390 MPa Show Material materials with Resistencia a la tracción of 320 - 390 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 460 J/(kg·K) Show Material materials with Calor específico of 460 J/(kg·K) | Typical for White Cast Iron |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 1/K | Typical for White Cast Iron |
Conductividad térmica | 20.0 °C | 14 W/(m·K) Show Material materials with Conductividad térmica of 14 W/(m·K) | |
Temperatura de fusión | 1209 °C Show Material materials with Temperatura de fusión of 1209 °C | Typical for White Cast Iron |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 8E-7 Ω·m Show Material materials with Resistividad eléctrica of 8E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbono | 2.6 - 2.9 % Show Material materials with Carbono of 2.6 - 2.9 % |
Cromo | 1.4 - 2.4 % Show Material materials with Cromo of 1.4 - 2.4 % |
Manganeso | 0.3 - 0.7 % Show Material materials with Manganeso of 0.3 - 0.7 % |
Molibdeno | 0.5 % Show Material materials with Molibdeno of 0.5 % |
Níquel | 3.3 - 5 % Show Material materials with Níquel of 3.3 - 5 % |
Silicona | 0.2 - 0.8 % Show Material materials with Silicona of 0.2 - 0.8 % |