General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | Typical for Chromium Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Chromium Steel |
Elongación | 20.0 °C | 11 - 14 % Show Material materials with Elongación of 11 - 14 % | |
Estricción | 20.0 °C | 40 - 50 % Show Material materials with Estricción of 40 - 50 % | |
Hardness, Rockwell F | 20.0 °C | 54 [-] Show Material materials with Hardness, Rockwell F of 54 [-] | |
Límite elástico | 20.0 °C | 560 - 780 MPa Show Material materials with Límite elástico of 560 - 780 MPa | |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Chromium Steel |
Resistencia a la tracción | 20.0 °C | 780 - 1180 MPa Show Material materials with Resistencia a la tracción of 780 - 1180 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 440 - 494 J/(kg·K) Show Material materials with Calor específico of 440 - 494 J/(kg·K) | Typical for Chromium Steel |
Coeficiente de dilatación térmica | 23.0 °C | 9.4E-6 - 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 9.4E-6 - 1.5E-5 1/K | Typical for Chromium Steel |
Conductividad térmica | 23.0 °C | 23 - 50 W/(m·K) Show Material materials with Conductividad térmica of 23 - 50 W/(m·K) | Typical for Chromium Steel |
Temperatura de fusión | 1382 - 1529 °C Show Material materials with Temperatura de fusión of 1382 - 1529 °C | Typical for Chromium Steel |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.38 - 0.44 % Show Material materials with Carbono of 0.38 - 0.44 % |
Cromo | 0.9 - 1.2 % Show Material materials with Cromo of 0.9 - 1.2 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.5 - 0.8 % Show Material materials with Manganeso of 0.5 - 0.8 % |
Silicona | 0.15 - 0.4 % Show Material materials with Silicona of 0.15 - 0.4 % |