General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.86 g/cm³ Show Material materials with Densidad of 7.86 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Tool And Machining Steel |
Módulo de cizallamiento | 23.0 °C | 79 GPa Show Material materials with Módulo de cizallamiento of 79 GPa | Typical for Tool And Machining Steel |
Módulo elástico | 20.0 °C | 207 GPa Show Material materials with Módulo elástico of 207 GPa | |
100.0 °C | 203 GPa Show Material materials with Módulo elástico of 203 GPa | ||
200.0 °C | 197 GPa Show Material materials with Módulo elástico of 197 GPa | ||
300.0 °C | 189 GPa Show Material materials with Módulo elástico of 189 GPa | ||
400.0 °C | 181 GPa Show Material materials with Módulo elástico of 181 GPa | ||
500.0 °C | 172 GPa Show Material materials with Módulo elástico of 172 GPa | ||
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 464 J/(kg·K) Show Material materials with Calor específico of 464 J/(kg·K) | |
100.0 °C | 479 J/(kg·K) Show Material materials with Calor específico of 479 J/(kg·K) | ||
200.0 °C | 496 J/(kg·K) Show Material materials with Calor específico of 496 J/(kg·K) | ||
300.0 °C | 513 J/(kg·K) Show Material materials with Calor específico of 513 J/(kg·K) | ||
400.0 °C | 532 J/(kg·K) Show Material materials with Calor específico of 532 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100.0 °C | 1.15E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.15E-5 1/K | |
200.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K | ||
300.0 °C | 1.24E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.24E-5 1/K | ||
400.0 °C | 1.28E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.28E-5 1/K | ||
500.0 °C | 1.31E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.31E-5 1/K | ||
600.0 °C | 1.35E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.35E-5 1/K | ||
Conductividad térmica | 20.0 °C | 32.9 W/(m·K) Show Material materials with Conductividad térmica of 32.9 W/(m·K) | |
100.0 °C | 34.2 W/(m·K) Show Material materials with Conductividad térmica of 34.2 W/(m·K) | ||
200.0 °C | 34.8 W/(m·K) Show Material materials with Conductividad térmica of 34.8 W/(m·K) | ||
300.0 °C | 34.4 W/(m·K) Show Material materials with Conductividad térmica of 34.4 W/(m·K) | ||
400.0 °C | 33.3 W/(m·K) Show Material materials with Conductividad térmica of 33.3 W/(m·K) | ||
Difusividad térmica | 20.0 °C | 9 mm²/s Show Material materials with Difusividad térmica of 9 mm²/s | |
100.0 °C | 8.8 mm²/s Show Material materials with Difusividad térmica of 8.8 mm²/s | ||
200.0 °C | 8.5 mm²/s Show Material materials with Difusividad térmica of 8.5 mm²/s | ||
300.0 °C | 7.8 mm²/s Show Material materials with Difusividad térmica of 7.8 mm²/s | ||
400.0 °C | 7.1 mm²/s Show Material materials with Difusividad térmica of 7.1 mm²/s | ||
Temperatura de fusión | 1370 - 1425 °C Show Material materials with Temperatura de fusión of 1370 - 1425 °C | Typical for Tool And Machining Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 3.17E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.17E-7 Ω·m |
100.0 °C | 3.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 3.74E-7 Ω·m | |
200.0 °C | 4.54E-7 Ω·m Show Material materials with Resistividad eléctrica of 4.54E-7 Ω·m | |
300.0 °C | 5.46E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.46E-7 Ω·m | |
400.0 °C | 6.53E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.53E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.4 - 0.5 % Show Material materials with Carbono of 0.4 - 0.5 % |
Cromo | 1.2 - 1.5 % Show Material materials with Cromo of 1.2 - 1.5 % |
Fósforo | 0.03 % Show Material materials with Fósforo of 0.03 % |
Manganeso | 0.15 - 0.45 % Show Material materials with Manganeso of 0.15 - 0.45 % |
Molibdeno | 0.15 - 0.35 % Show Material materials with Molibdeno of 0.15 - 0.35 % |
Níquel | 3.8 - 4.3 % Show Material materials with Níquel of 3.8 - 4.3 % |
Silicona | 0.1 - 0.4 % Show Material materials with Silicona of 0.1 - 0.4 % |
Wolframio | 0.4 - 0.6 % Show Material materials with Wolframio of 0.4 - 0.6 % |