Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Soft Magnetic Iron |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 470 J/(kg·K) Show Material materials with Calor específico of 470 J/(kg·K) | Typical for Soft Magnetic Iron |
Coeficiente de dilatación térmica | 23.0 °C | 2E-6 - 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 2E-6 - 1.2E-5 1/K | Typical for Soft Magnetic Iron |
Conductividad térmica | 23.0 °C | 13 - 55 W/(m·K) Show Material materials with Conductividad térmica of 13 - 55 W/(m·K) | Typical for Soft Magnetic Iron |
Technological properties
Property | ||
---|---|---|
Features | Soft magnetic |