General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 7.3 g/cm³ Show Material materials with Densidad of 7.3 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Ferritic Stainless Steel |
Elongación | 20.0 °C | 8 % Show Material materials with Elongación of 8 % | |
Elongation A100 | 20.0 °C | 8 - 18 % Show Material materials with Elongation A100 of 8 - 18 % | |
Módulo de cizallamiento | 23.0 °C | 77 GPa Show Material materials with Módulo de cizallamiento of 77 GPa | Typical for Ferritic Stainless Steel |
Módulo elástico | 23.0 °C | 220 GPa Show Material materials with Módulo elástico of 220 GPa | Typical for Ferritic Stainless Steel |
Resistencia a la tracción | 20.0 °C | 600 MPa Show Material materials with Resistencia a la tracción of 600 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 480 J/(kg·K) Show Material materials with Calor específico of 480 J/(kg·K) | |
1000.0 °C | 650 J/(kg·K) Show Material materials with Calor específico of 650 J/(kg·K) | ||
Coeficiente de dilatación térmica | 200.0 °C | 1.1E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 1/K | |
400.0 °C | 1.2E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.2E-5 1/K | ||
600.0 °C | 1.3E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.3E-5 1/K | ||
800.0 °C | 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.4E-5 1/K | ||
1000.0 °C | 1.5E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 1/K | ||
Conductividad térmica | 20.0 °C | 15 W/(m·K) Show Material materials with Conductividad térmica of 15 W/(m·K) | |
Temperatura de fusión | 1425 - 1530 °C Show Material materials with Temperatura de fusión of 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Temperatura máx. de funcionamiento, largo | 1250 - 1350 °C Show Material materials with Temperatura máx. de funcionamiento, largo of 1250 - 1350 °C |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 1.25E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.25E-6 Ω·m |
100.0 °C | 1.26E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.26E-6 Ω·m | |
200.0 °C | 1.27E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.27E-6 Ω·m | |
300.0 °C | 1.28E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.28E-6 Ω·m | |
400.0 °C | 1.3E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.3E-6 Ω·m | |
500.0 °C | 1.32E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.32E-6 Ω·m | |
600.0 °C | 1.34E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.34E-6 Ω·m | |
700.0 °C | 1.36E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.36E-6 Ω·m | |
800.0 °C | 1.39E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.39E-6 Ω·m | |
900.0 °C | 1.41E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.41E-6 Ω·m | |
1000.0 °C | 1.42E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.42E-6 Ω·m | |
1100.0 °C | 1.44E-6 Ω·m Show Material materials with Resistividad eléctrica of 1.44E-6 Ω·m | |
Chemical properties
Property | Value |
---|---|
Aluminio | 3.5 - 5 % Show Material materials with Aluminio of 3.5 - 5 % |
Azufre | 0.03 % Show Material materials with Azufre of 0.03 % |
Carbono | 0.1 % Show Material materials with Carbono of 0.1 % |
Cromo | 13 - 15 % Show Material materials with Cromo of 13 - 15 % |
Fósforo | 0.05 % Show Material materials with Fósforo of 0.05 % |
Manganeso | 1 % Show Material materials with Manganeso of 1 % |
Silicona | 0.5 % Show Material materials with Silicona of 0.5 % |