General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.3 g/cm³ Show Material materials with Densidad of 8.3 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 80 [-] Show Material materials with Dureza Brinell of 80 [-] |
Elongación | 20.0 °C | 12 % Show Material materials with Elongación of 12 % |
Límite elástico Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Límite elástico Rp 0,2 of 120 MPa |
Módulo elástico | 20.0 °C | 152 GPa Show Material materials with Módulo elástico of 152 GPa |
Resistencia a la tracción | 20.0 °C | 320 MPa Show Material materials with Resistencia a la tracción of 320 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 430 - 532 J/(kg·K) Show Material materials with Calor específico of 430 - 532 J/(kg·K) | Typical for Pure/Low Nickel Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 8.5E-6 - 1.4E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 8.5E-6 - 1.4E-5 1/K | Typical for Pure/Low Nickel Alloy |
Conductividad térmica | 23.0 °C | 18 - 86 W/(m·K) Show Material materials with Conductividad térmica of 18 - 86 W/(m·K) | Typical for Pure/Low Nickel Alloy |
Temperatura de fusión | 1400 - 1500 °C Show Material materials with Temperatura de fusión of 1400 - 1500 °C | Typical for Pure/Low Nickel Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 2.85E-7 Ω·m Show Material materials with Resistividad eléctrica of 2.85E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Carbono | 1 % Show Material materials with Carbono of 1 % |
Cobre | 1.2 % Show Material materials with Cobre of 1.2 % |
Hierro | 1 % Show Material materials with Hierro of 1 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 95 % Show Material materials with Níquel of 95 % |
Silicona | 2 % Show Material materials with Silicona of 2 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting, separately cast test sample |