General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.4 g/cm³ Show Material materials with Densidad of 8.4 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 20.0 °C | 260 [-] Show Material materials with Dureza Brinell of 260 [-] | |
Elongación | 20.0 °C | 1 % Show Material materials with Elongación of 1 % | |
Límite elástico Rp 0,2 | 20.0 °C | 500 MPa Show Material materials with Límite elástico Rp 0,2 of 500 MPa | |
Módulo elástico | 23.0 °C | 120 - 156 GPa Show Material materials with Módulo elástico of 120 - 156 GPa | Typical for Nickel Copper Alloy |
Resistencia a la tracción | 20.0 °C | 750 MPa Show Material materials with Resistencia a la tracción of 750 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 418 - 540 J/(kg·K) Show Material materials with Calor específico of 418 - 540 J/(kg·K) | Typical for Nickel Copper Alloy |
Coeficiente de dilatación térmica | 23.0 °C | 1.1E-5 - 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.1E-5 - 1.6E-5 1/K | Typical for Nickel Copper Alloy |
Conductividad térmica | 23.0 °C | 16 - 45 W/(m·K) Show Material materials with Conductividad térmica of 16 - 45 W/(m·K) | Typical for Nickel Copper Alloy |
Temperatura de fusión | 1170 - 1365 °C Show Material materials with Temperatura de fusión of 1170 - 1365 °C | Typical for Nickel Copper Alloy |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Azufre | 0.01 % Show Material materials with Azufre of 0.01 % |
Carbono | 0.25 % Show Material materials with Carbono of 0.25 % |
Cobre | 27 - 31 % Show Material materials with Cobre of 27 - 31 % |
Hierro | 1 - 2.5 % Show Material materials with Hierro of 1 - 2.5 % |
Magnesio | 0.12 % Show Material materials with Magnesio of 0.12 % |
Manganeso | 0.5 - 1.5 % Show Material materials with Manganeso of 0.5 - 1.5 % |
Níquel | 60 - 68 % Show Material materials with Níquel of 60 - 68 % |
Plomo | 0.01 % Show Material materials with Plomo of 0.01 % |
Silicona | 3.5 - 4.5 % Show Material materials with Silicona of 3.5 - 4.5 % |
Titanio | 0.2 % Show Material materials with Titanio of 0.2 % |
Technological properties
Property | ||
---|---|---|
Processing methods | sand casting, separately cast test sample |