DIN 17741 Grade Ni99.4Fe

Want to keep this datasheet? Save it now in your required format

Description

Ni99.4Fe is a resistance alloy. With wire, the attainable tensile strength is 450 N/mm². The alloy distinguishes itself by a very high and exactly defined temperature coefficient of the electric resistance that is standardized according to DIN 43760. The upper application temperature in air is 750 °C, and it is 250 degrees C in case of an application for electric resistance thermometers according to DIN 43760. Ni99.4Fe can be soft-soldered and brazed without difficulty. All known welding methods are applicable. Application: Exclusively for the manufacturing of temperature-sensitive elements and electric resistance thermometers.

Related Standards

Equivalent Materials

Los datos sobre este material han sido proporcionados por WIAM.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyTemperatureValue

Densidad

20.0 °C

8.9 g/cm³

Show Material materials with Densidad of 8.9 g/cm³

Mecánica

PropertyTemperatureValueComment

Módulo elástico

23.0 °C

190 - 220 GPa

Show Material materials with Módulo elástico of 190 - 220 GPa

Typical for Pure/Low Nickel Alloy

Aplicaciones térmicas

PropertyTemperatureValueComment

Calor específico

20.0 °C

470 J/(kg·K)

Show Material materials with Calor específico of 470 J/(kg·K)

Coeficiente de dilatación térmica

23.0 °C

8.5E-6 - 1.4E-5 1/K

Show Material materials with Coeficiente de dilatación térmica of 8.5E-6 - 1.4E-5 1/K

Typical for Pure/Low Nickel Alloy

Conductividad térmica

20.0 °C

70 W/(m·K)

Show Material materials with Conductividad térmica of 70 W/(m·K)

Temperatura de fusión

1400 - 1500 °C

Show Material materials with Temperatura de fusión of 1400 - 1500 °C

Typical for Pure/Low Nickel Alloy

Temperatura máx. de funcionamiento, largo

0 - 750 °C

Show Material materials with Temperatura máx. de funcionamiento, largo of 0 - 750 °C

Eléctrico

PropertyTemperatureValue

Resistividad eléctrica

20.0 °C

7.6E-8 Ω·m

Show Material materials with Resistividad eléctrica of 7.6E-8 Ω·m

Chemical properties

PropertyValue

Azufre

5E-3 %

Show Material materials with Azufre of 5E-3 %

Carbono

0.05 %

Show Material materials with Carbono of 0.05 %

Cobalto

1 %

Show Material materials with Cobalto of 1 %

Cobre

0.05 %

Show Material materials with Cobre of 0.05 %

Hierro

0.2 - 0.6 %

Show Material materials with Hierro of 0.2 - 0.6 %

Magnesio

0.05 %

Show Material materials with Magnesio of 0.05 %

Manganeso

0.05 %

Show Material materials with Manganeso of 0.05 %

Níquel

98.4 %

Show Material materials with Níquel of 98.4 %

Silicona

0.02 %

Show Material materials with Silicona of 0.02 %