General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.8 g/cm³ Show Material materials with Densidad of 8.8 g/cm³ |
Mecánica
Property | Temperature | Value |
---|---|---|
Dureza Brinell | 20.0 °C | 120 - 140 [-] Show Material materials with Dureza Brinell of 120 - 140 [-] |
Elongación | 20.0 °C | 35 % Show Material materials with Elongación of 35 % |
Elongation A100 | 20.0 °C | 20 - 30 % Show Material materials with Elongation A100 of 20 - 30 % |
Límite elástico Rp 0,2 | 20.0 °C | 160 MPa Show Material materials with Límite elástico Rp 0,2 of 160 MPa |
Límite elástico Rp 1,0 | 20.0 °C | 185 MPa Show Material materials with Límite elástico Rp 1,0 of 185 MPa |
Módulo elástico | 20.0 °C | 182 GPa Show Material materials with Módulo elástico of 182 GPa |
100.0 °C | 180 GPa Show Material materials with Módulo elástico of 180 GPa | |
200.0 °C | 177 GPa Show Material materials with Módulo elástico of 177 GPa | |
300.0 °C | 170 GPa Show Material materials with Módulo elástico of 170 GPa | |
400.0 °C | 165 GPa Show Material materials with Módulo elástico of 165 GPa | |
500.0 °C | 150 GPa Show Material materials with Módulo elástico of 150 GPa | |
Resistencia a la tracción | 20.0 °C | 400 - 500 MPa Show Material materials with Resistencia a la tracción of 400 - 500 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 20.0 °C | 427 J/(kg·K) Show Material materials with Calor específico of 427 J/(kg·K) | |
100.0 °C | 445 J/(kg·K) Show Material materials with Calor específico of 445 J/(kg·K) | ||
200.0 °C | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | ||
300.0 °C | 478 J/(kg·K) Show Material materials with Calor específico of 478 J/(kg·K) | ||
400.0 °C | 490 J/(kg·K) Show Material materials with Calor específico of 490 J/(kg·K) | ||
Coeficiente de dilatación térmica | 100.0 °C | 1.39E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.39E-5 1/K | |
200.0 °C | 1.55E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.55E-5 1/K | ||
300.0 °C | 1.58E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.58E-5 1/K | ||
400.0 °C | 1.6E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 1/K | ||
500.0 °C | 1.63E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.63E-5 1/K | ||
600.0 °C | 1.66E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.66E-5 1/K | ||
700.0 °C | 1.7E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.7E-5 1/K | ||
800.0 °C | 1.74E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.74E-5 1/K | ||
900.0 °C | 1.77E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.77E-5 1/K | ||
Conductividad térmica | 20.0 °C | 21.8 W/(m·K) Show Material materials with Conductividad térmica of 21.8 W/(m·K) | |
100.0 °C | 29.5 W/(m·K) Show Material materials with Conductividad térmica of 29.5 W/(m·K) | ||
200.0 °C | 33 W/(m·K) Show Material materials with Conductividad térmica of 33 W/(m·K) | ||
300.0 °C | 36.5 W/(m·K) Show Material materials with Conductividad térmica of 36.5 W/(m·K) | ||
400.0 °C | 40 W/(m·K) Show Material materials with Conductividad térmica of 40 W/(m·K) | ||
500.0 °C | 44 W/(m·K) Show Material materials with Conductividad térmica of 44 W/(m·K) | ||
600.0 °C | 48.5 W/(m·K) Show Material materials with Conductividad térmica of 48.5 W/(m·K) | ||
700.0 °C | 52 W/(m·K) Show Material materials with Conductividad térmica of 52 W/(m·K) | ||
800.0 °C | 56 W/(m·K) Show Material materials with Conductividad térmica of 56 W/(m·K) | ||
900.0 °C | 58 W/(m·K) Show Material materials with Conductividad térmica of 58 W/(m·K) | ||
Temperatura de fusión | 1170 - 1365 °C Show Material materials with Temperatura de fusión of 1170 - 1365 °C | Typical for Nickel Copper Alloy |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 5.47E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.47E-7 Ω·m |
100.0 °C | 5.4E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.4E-7 Ω·m | |
200.0 °C | 5.55E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.55E-7 Ω·m | |
300.0 °C | 5.75E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.75E-7 Ω·m | |
400.0 °C | 5.85E-7 Ω·m Show Material materials with Resistividad eléctrica of 5.85E-7 Ω·m | |
500.0 °C | 6E-7 Ω·m Show Material materials with Resistividad eléctrica of 6E-7 Ω·m | |
600.0 °C | 6.18E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.18E-7 Ω·m | |
700.0 °C | 6.35E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.35E-7 Ω·m | |
800.0 °C | 6.55E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.55E-7 Ω·m | |
900.0 °C | 6.75E-7 Ω·m Show Material materials with Resistividad eléctrica of 6.75E-7 Ω·m | |
Chemical properties
Property | Value |
---|---|
Aluminio | 0.5 % Show Material materials with Aluminio of 0.5 % |
Azufre | 0.02 % Show Material materials with Azufre of 0.02 % |
Carbono | 0.04 % Show Material materials with Carbono of 0.04 % |
Cobalto | 1 % Show Material materials with Cobalto of 1 % |
Cobre | 28 - 34 % Show Material materials with Cobre of 28 - 34 % |
Hierro | 1 - 2.5 % Show Material materials with Hierro of 1 - 2.5 % |
Manganeso | 2 % Show Material materials with Manganeso of 2 % |
Níquel | 62 % Show Material materials with Níquel of 62 % |
Silicona | 0.3 % Show Material materials with Silicona of 0.3 % |
Titanio | 0.3 % Show Material materials with Titanio of 0.3 % |