General
Property | Temperature | Value |
---|---|---|
Densidad | 20.0 °C | 8.15 g/cm³ Show Material materials with Densidad of 8.15 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | Typical for Nickel Steel |
Módulo de cizallamiento | 23.0 °C | 76 GPa Show Material materials with Módulo de cizallamiento of 76 GPa | Typical for Nickel Steel |
Módulo elástico | 23.0 °C | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | Typical for Nickel Steel |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 456 J/(kg·K) Show Material materials with Calor específico of 456 J/(kg·K) | Typical for Nickel Steel |
Conductividad térmica | 23.0 °C | 10 - 50 W/(m·K) Show Material materials with Conductividad térmica of 10 - 50 W/(m·K) | Typical for Nickel Steel |
Temperatura de fusión | 1316 - 1595 °C Show Material materials with Temperatura de fusión of 1316 - 1595 °C | Typical for Nickel Steel |
Eléctrico
Property | Temperature | Value |
---|---|---|
Resistividad eléctrica | 20.0 °C | 7.5E-7 Ω·m Show Material materials with Resistividad eléctrica of 7.5E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Níquel | 36 - 40 % Show Material materials with Níquel of 36 - 40 % |