General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.8 g/cm³ Show Material materials with Densidad of 7.8 g/cm³ | Typical for Steel |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.3 [-] Show Material materials with Coeficiente de Poisson of 0.3 [-] | Typical for Steel |
Elongación | 20.0 °C | 22 % Show Material materials with Elongación of 22 % | |
Límite elástico | 20.0 °C | 355 MPa Show Material materials with Límite elástico of 355 MPa | |
Límite elástico Rp 0,2 | 100.0 °C | 255 MPa Show Material materials with Límite elástico Rp 0,2 of 255 MPa | |
200.0 °C | 226 MPa Show Material materials with Límite elástico Rp 0,2 of 226 MPa | ||
250.0 °C | 206 MPa Show Material materials with Límite elástico Rp 0,2 of 206 MPa | ||
300.0 °C | 186 MPa Show Material materials with Límite elástico Rp 0,2 of 186 MPa | ||
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | Typical for Steel |
Resistencia a la tracción | 20.0 °C | 510 - 610 MPa Show Material materials with Resistencia a la tracción of 510 - 610 MPa |
Chemical properties
Property | Value |
---|---|
Azufre | 0.035 % Show Material materials with Azufre of 0.035 % |
Carbono | 0.12 % Show Material materials with Carbono of 0.12 % |
Cobre | 0.25 - 0.55 % Show Material materials with Cobre of 0.25 - 0.55 % |
Cromo | 0.5 - 1.25 % Show Material materials with Cromo of 0.5 - 1.25 % |
Fósforo | 0.07 - 0.15 % Show Material materials with Fósforo of 0.07 - 0.15 % |
Manganeso | 0.2 - 0.5 % Show Material materials with Manganeso of 0.2 - 0.5 % |
Níquel | 0.65 % Show Material materials with Níquel of 0.65 % |
Silicona | 0.25 - 0.75 % Show Material materials with Silicona of 0.25 - 0.75 % |