General
Property | Temperature | Value |
---|---|---|
Densidad | 23.0 °C | 7.85 g/cm³ Show Material materials with Densidad of 7.85 g/cm³ |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.27 [-] Show Material materials with Coeficiente de Poisson of 0.27 [-] | In Normalized Condition |
Dureza Brinell | 23.0 °C | 197 [-] Show Material materials with Dureza Brinell of 197 [-] | |
Dureza Rockwell B | 23.0 °C | 92 [-] Show Material materials with Dureza Rockwell B of 92 [-] | |
Elongación | 23.0 °C | 7 - 18 % Show Material materials with Elongación of 7 - 18 % | For Different Conditions |
Límite elástico | 23.0 °C | 560 MPa Show Material materials with Límite elástico of 560 MPa | |
Módulo de cizallamiento | 23.0 °C | 75 - 80 GPa Show Material materials with Módulo de cizallamiento of 75 - 80 GPa | Typical for Carbon Steel |
Módulo elástico | 23.0 °C | 190 - 210 GPa Show Material materials with Módulo elástico of 190 - 210 GPa | In Normalized Condition |
Resistencia a la tracción | 23.0 °C | 630 - 950 MPa Show Material materials with Resistencia a la tracción of 630 - 950 MPa | For Different Conditions |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 470 - 520 J/(kg·K) Show Material materials with Calor específico of 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Coeficiente de dilatación térmica | 23.0 °C | 1.32E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32E-5 1/K | Typical for Medium Carbon Steel |
Conductividad térmica | 23.0 °C | 21 - 52 W/(m·K) Show Material materials with Conductividad térmica of 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Temperatura de fusión | 1380 - 1514 °C Show Material materials with Temperatura de fusión of 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | Typical for Carbon Steel |
Eléctrico
Property | Temperature | Value | Comment |
---|---|---|---|
Resistividad eléctrica | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m Show Material materials with Resistividad eléctrica of 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
Property | Value |
---|---|
Carbono | 0.5 - 0.6 % Show Material materials with Carbono of 0.5 - 0.6 % |
Manganeso | 0.6 - 0.9 % Show Material materials with Manganeso of 0.6 - 0.9 % |
Technological properties
Property | ||
---|---|---|
Corrosion properties | Not Corrosion Resistance |