Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Charpy impact energy, V-notch | -12 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J | average |
4 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J | average | |
21 °C | 27 J Show Material materials with Charpy impact energy, V-notch of 27 J | average | |
Elongación | 18 - 21 % Show Material materials with Elongación of 18 - 21 % | ||
Resistencia a la tracción | 485 MPa Show Material materials with Resistencia a la tracción of 485 MPa | min. |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.01 - 0.04 % Show Material materials with Aluminio of 0.01 - 0.04 % | |
Azufre | 0.006 % Show Material materials with Azufre of 0.006 % | max. |
Carbono | 0.11 % Show Material materials with Carbono of 0.11 % | max. |
Cobre | 0.25 - 0.4 % Show Material materials with Cobre of 0.25 - 0.4 % | |
Cromo | 0.45 - 0.7 % Show Material materials with Cromo of 0.45 - 0.7 % | |
Fósforo | 0.2 % Show Material materials with Fósforo of 0.2 % | max. |
Manganeso | 1.1 - 1.5 % Show Material materials with Manganeso of 1.1 - 1.5 % | |
Molibdeno | 0.02 - 0.08 % Show Material materials with Molibdeno of 0.02 - 0.08 % | |
Nitrógeno | 0.015 % Show Material materials with Nitrógeno of 0.015 % | max. |
Níquel | 0.25 - 0.4 % Show Material materials with Níquel of 0.25 - 0.4 % | |
Silicona | 0.3 - 0.5 % Show Material materials with Silicona of 0.3 - 0.5 % | |
Vanadio | 0.04 - 0.08 % Show Material materials with Vanadio of 0.04 - 0.08 % |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |