General
Property | Value | Comment |
---|---|---|
Densidad | 7.8 - 7.9 g/cm³ Show Material materials with Densidad of 7.8 - 7.9 g/cm³ | typical for low carbon steel |
Mecánica
Property | Value | Comment |
---|---|---|
Coeficiente de Poisson | 0.29 [-] Show Material materials with Coeficiente de Poisson of 0.29 [-] | typical for low carbon steel |
Elongación | 20 - 22 % Show Material materials with Elongación of 20 - 22 % | min. values depending on the thickness |
Límite elástico | 315 - 415 MPa Show Material materials with Límite elástico of 315 - 415 MPa | ReH, min. values depending on the thickness, If not apparent, the yield strength Rp0.2 is measured |
Módulo de cizallamiento | 82 GPa Show Material materials with Módulo de cizallamiento of 82 GPa | typical for low carbon steel |
Módulo elástico | 200 - 215 GPa Show Material materials with Módulo elástico of 200 - 215 GPa | typical for low carbon steel |
Resistencia a la tracción | 485 - 690 MPa Show Material materials with Resistencia a la tracción of 485 - 690 MPa | range depending on the thickness |
Aplicaciones térmicas
Property | Value | Comment |
---|---|---|
Calor específico | 465 J/(kg·K) Show Material materials with Calor específico of 465 J/(kg·K) | typical for low carbon steel |
Coeficiente de dilatación térmica | 1.32e-05 - 1.38e-05 1/K Show Material materials with Coeficiente de dilatación térmica of 1.32e-05 - 1.38e-05 1/K | typical for low carbon steel |
Conductividad térmica | 25 - 93 W/(m·K) Show Material materials with Conductividad térmica of 25 - 93 W/(m·K) | typical for low carbon steel |
Temperatura de fusión | 1480 - 1526 °C Show Material materials with Temperatura de fusión of 1480 - 1526 °C | typical for low carbon steel |
Temperatura máx. de funcionamiento | 500 °C Show Material materials with Temperatura máx. de funcionamiento of 500 °C | typical for carbon steel |
Eléctrico
Property | Value | Comment |
---|---|---|
Resistividad eléctrica | 1.43e-07 - 1.74e-07 Ω·m Show Material materials with Resistividad eléctrica of 1.43e-07 - 1.74e-07 Ω·m | typical for carbon steel |
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Material materials with Azufre of 0.025 % | max. |
Carbono | 0.24 % Show Material materials with Carbono of 0.24 % | |
Cobre | 0.35 - 0.38 % Show Material materials with Cobre of 0.35 - 0.38 % | depending on analysis |
Cromo | 0.25 - 0.29 % Show Material materials with Cromo of 0.25 - 0.29 % | depending on analysis |
Fósforo | 0.025 % Show Material materials with Fósforo of 0.025 % | max. |
Manganeso | 0.64 - 1.72 % Show Material materials with Manganeso of 0.64 - 1.72 % | depending on analysis and thickness |
Molibdeno | 0.08 - 0.09 % Show Material materials with Molibdeno of 0.08 - 0.09 % | depending on analysis |
Níquel | 0.25 - 0.28 % Show Material materials with Níquel of 0.25 - 0.28 % | depending on analysis |
Silicona | 0.13 - 0.55 % Show Material materials with Silicona of 0.13 - 0.55 % | depending on analysis |
Technological properties
Property | ||
---|---|---|
Supplier Disclaimer | The given information is a rough description and some properties can depend on various factors such as product thickness. Please contact the supplier or refer to the related norm or standard for further information. |