Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 10 % Show Material materials with Elongación A50 of 10 % |
Límite elástico Rp0.5 | 20.0 °C | 345 MPa Show Material materials with Límite elástico Rp0.5 of 345 MPa |
Resistencia a la tracción | 20.0 °C | 690 MPa Show Material materials with Resistencia a la tracción of 690 MPa |
Chemical properties
Property | Value |
---|---|
Aluminio | 9 - 11 % Show Material materials with Aluminio of 9 - 11 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 2 - 4 % Show Material materials with Hierro of 2 - 4 % |
Manganeso | 1.5 % Show Material materials with Manganeso of 1.5 % |
Níquel | 4 - 5.5 % Show Material materials with Níquel of 4 - 5.5 % |
Silicona | 0.25 % Show Material materials with Silicona of 0.25 % |
Zinc | 0.3 % Show Material materials with Zinc of 0.3 % |