General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Densidad of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.33 [-] Show Material materials with Coeficiente de Poisson of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Dureza Rockwell B | 23.0 °C | 70 - 100 [-] Show Material materials with Dureza Rockwell B of 70 - 100 [-] | |
Elongación A50 | 23.0 °C | 9 - 15 % Show Material materials with Elongación A50 of 9 - 15 % | |
Límite elástico Rp0.5 | 23.0 °C | 240 - 310 MPa Show Material materials with Límite elástico Rp0.5 of 240 - 310 MPa | |
Módulo elástico | 23.0 °C | 110 - 130 GPa Show Material materials with Módulo elástico of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Resistencia a la tracción | 23.0 °C | 515 - 620 MPa Show Material materials with Resistencia a la tracción of 515 - 620 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 380 J/(kg·K) Show Material materials with Calor específico of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Coeficiente de dilatación térmica | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminio | 6.3 - 7.6 % Show Material materials with Aluminio of 6.3 - 7.6 % |
Arsénico | 0.09 % Show Material materials with Arsénico of 0.09 % |
Estaño | 0.2 % Show Material materials with Estaño of 0.2 % |
Hierro | 0.3 % Show Material materials with Hierro of 0.3 % |
Manganeso | 0.1 % Show Material materials with Manganeso of 0.1 % |
Níquel | 0.25 % Show Material materials with Níquel of 0.25 % |
Plomo | 0.05 % Show Material materials with Plomo of 0.05 % |
Silicona | 1.5 - 2.2 % Show Material materials with Silicona of 1.5 - 2.2 % |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % |