General
Property | Temperature | Value | Comment |
---|---|---|---|
Densidad | 23.0 °C | 8.9 g/cm³ Show Material materials with Densidad of 8.9 g/cm³ | Typical for Wrought Copper Pure / Low Alloyed Copper |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Coeficiente de Poisson | 23.0 °C | 0.34 [-] Show Material materials with Coeficiente de Poisson of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Hardness, Rockwell F | 23.0 °C | 86 - 93 [-] Show Material materials with Hardness, Rockwell F of 86 - 93 [-] | |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 54 - 62 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 54 - 62 [-] | |
Módulo de cizallamiento | 23.0 °C | 48 GPa Show Material materials with Módulo de cizallamiento of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Módulo elástico | 23.0 °C | 95 - 98 GPa Show Material materials with Módulo elástico of 95 - 98 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Resistencia a la tracción | 23.0 °C | 295 - 360 MPa Show Material materials with Resistencia a la tracción of 295 - 360 MPa |
Aplicaciones térmicas
Property | Temperature | Value | Comment |
---|---|---|---|
Calor específico | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Calor específico of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Coeficiente de dilatación térmica | 23.0 °C | 1.6E-5 - 1.8E-5 1/K Show Material materials with Coeficiente de dilatación térmica of 1.6E-5 - 1.8E-5 1/K | Typical for Wrought Copper Pure / Low Alloyed Copper |
Temperatura de fusión | 965 - 1100 °C Show Material materials with Temperatura de fusión of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper |
Chemical properties
Property | Value |
---|---|
Cobre | 99.9 % Show Material materials with Cobre of 99.9 % |
Estaño | 0 - 0.02 % Show Material materials with Estaño of 0 - 0.02 % |
Fósforo | 0 - 0.01 % Show Material materials with Fósforo of 0 - 0.01 % |
Telurio | 0 - 0.02 % Show Material materials with Telurio of 0 - 0.02 % |