Mecánica
Property | Temperature | Value |
---|---|---|
Elongación A50 | 20.0 °C | 35 % Show Material materials with Elongación A50 of 35 % |
Límite elástico Rp0.5 | 20.0 °C | 105 MPa Show Material materials with Límite elástico Rp0.5 of 105 MPa |
Resistencia a la tracción | 20.0 °C | 310 MPa Show Material materials with Resistencia a la tracción of 310 MPa |
Yield Strength Rp0.2, short transverse | 20.0 °C | 105 MPa Show Material materials with Yield Strength Rp0.2, short transverse of 105 MPa |
Chemical properties
Property | Value |
---|---|
Cobre | 70 - 73 % Show Material materials with Cobre of 70 - 73 % |
Estaño | 0.8 - 1.2 % Show Material materials with Estaño of 0.8 - 1.2 % |
Hierro | 0.06 % Show Material materials with Hierro of 0.06 % |
Plomo | 0.07 % Show Material materials with Plomo of 0.07 % |